Other Blogs
ASA, if your printer has an enclosure. It survives direct sunlight for years, handles summer heat and stays tough in winter. On an open printer, use PCTG or PETG. Don't use PLA: it softens on a hot day and breaks down in the sun.
Outdoors a part has to survive three things: UV light, heat and cold. Here's how the usual candidates handle each one:
| Sunlight | Summer heat | Cold and knocks | Easy to print | |
|---|---|---|---|---|
| ASA | Good Keeps its color and strength | Good HDT 86–96 °C | Good As tough as ABS | Poor Enclosure, fumes |
| PC-PBT | No data Not rated | Good HDT 107 °C | Good Rated down to −30 °C | Poor Enclosure, 260 °C nozzle |
| PCTG | Good More weather resistant than PETG | OK HDT 76 °C | Good Very high impact strength | Good No enclosure |
| PETG | Good Fine in sunlight | OK Up to about 80 °C | OK Can crack when dropped | Good No enclosure |
| ABS | OK Yellows, still lasts years | Good About 100 °C | Good Stays tough in winter | Poor Warps, fumes |
| PC | Poor Degrades unless coated | Good Softens near 150 °C | Good Doesn't shatter | Poor Enclosure, hot nozzle |
| PLA | Poor Breaks down in sunlight | Poor Softens above 60 °C | Poor Shatters when dropped | Good Easiest of all |
In Zack Freedman's filament tier list, ASA is A tier and the outdoor pick. It's a chemical cousin of ABS with the weak spots fixed: as tough as ABS, it survives in direct sunlight indefinitely, it takes heat up to around the boiling point of water and it warps less. Polymaker's guide is just as clear: ASA "retains its color and mechanical properties even after prolonged sun exposure".
The price is the printing. ASA wants an enclosure (Polymaker suggests a 60 °C chamber), a 240–280 °C nozzle, a 90–110 °C bed, and it gives off the same styrene fumes as ABS. Print it in a ventilated room. If you're designing parts to fit, it also shrinks: see ASA shrinkage.
No enclosure? PETG handles sunlight well (Polymaker calls it ideal for outdoor use) and holds its shape up to about 80 °C. Its weak spots are impacts and sagging overhangs.
PCTG fixes both. Proto-pasta found it "more impact, chemical, and weather resistant than PETG", and it's the top of Zack's S tier. It costs more. Compare the two in PCTG vs PETG.
Both are polyesters with heat limits in the 70s and low 80s °C, so neither belongs on a car dashboard in summer.
Most plastics turn brittle in the cold. PC-PBT is one of very few filaments that stays tough well below freezing. Polymaker rates its PC-PBT's impact strength at −30 °C. Zack put it in A tier, "A for Arctic".
It's a polycarbonate blend, so it also takes heat (heat deflection at 107 °C). It prints at 260–280 °C, and Polymaker's data sheet calls for an enclosure. Use it for ski and snow gear, car parts or anything that lives outside through winter.
ABS works outdoors. Zack says it doesn't go brittle in winter, doesn't turn to taffy in summer and can take sunlight for most of a decade. Polymaker rates its UV resistance as poor. Either way, ASA does the same job with fewer problems, which is why Zack puts ABS in C tier.
PC takes the most heat of the common filaments (it softens near 150 °C), but plain polycarbonate degrades in sunlight unless you coat or paint it. Use it where heat matters more than sun, like near an engine or a lamp.
PLA softens above about 60 °C (a parked car gets hotter than that), UV light breaks it down and it shatters when dropped. It's fine for a garden gnome in the shade for a season. For anything that has to last, use one of the above.
There's one exception worth knowing: Polymaker says its weather-tested Matte PLA for Production performed on par with ASA in its tests. That's one specific product, not PLA in general, and it doesn't fix the heat problem.
Describe the part and where it goes. GrandpaCAD builds a parametric model you can resize, and can slice it for your printer.
Something for the garden, the bike or the car?
Describe it and name the filament.
ASA. It resists UV light, handles heat up to around 90–100 °C and stays tough in the cold. It needs an enclosed printer. Without one, PCTG or PETG are the best options.
Yes, reasonably. Polymaker lists PETG as suitable for UV-exposed outdoor parts. It softens at about 80 °C, so keep it away from very hot spots, and PCTG holds up better against impacts and weather.
Only for short-lived, decorative parts in the shade. PLA softens above about 60 °C, degrades in sunlight and becomes brittle.
PC-PBT. Polymaker rates it for impacts at −30 °C, and Zack Freedman ranks it A tier for exactly that reason. ASA and ABS also stay tough in winter.
Tiers and quotes from Zack Freedman's The 3D Filament Tier List! (Voidstar Lab, 2024). Material data from Polymaker's guides to ASA, PETG, PLA and PC, its PC-PBT data sheet and weather test, Fiberlogy PCTG and Proto-pasta.